Page 106
... reaction in dearated aqueous solutions can be associated to the hydrogen reduction reaction due to the large activation energy required by the recombination of adsorbed hydrogen atoms to produce molecular hydrogen ( Bockris and Reddy ...
... reaction in dearated aqueous solutions can be associated to the hydrogen reduction reaction due to the large activation energy required by the recombination of adsorbed hydrogen atoms to produce molecular hydrogen ( Bockris and Reddy ...
Page 108
O , OH он Cathodic reaction Anaerobic Corrosion 02 • 2 Fe 20 , 5H20 → 2 Fe ( OH ) , · 4H ' OH O2 · Fe → Fe ··· 2e " Anodic reaction HS HS Fe HS • HS FeS H · HS HS он он So • So H2O 2e -HS . OH · Fe - Fe · 2e Cathodic reaction Anodic ...
O , OH он Cathodic reaction Anaerobic Corrosion 02 • 2 Fe 20 , 5H20 → 2 Fe ( OH ) , · 4H ' OH O2 · Fe → Fe ··· 2e " Anodic reaction HS HS Fe HS • HS FeS H · HS HS он он So • So H2O 2e -HS . OH · Fe - Fe · 2e Cathodic reaction Anodic ...
Page 221
... reaction and enables the decomposition of vanadates . According to Logan , the reaction is : 14 V2O5 + 20 NaVO3 → 2 ( 5 Na2O , V2O4 , 11 V205 ) + O2 C. Dissolution of oxygen in the molten mixture . According to Cunningham and De S ...
... reaction and enables the decomposition of vanadates . According to Logan , the reaction is : 14 V2O5 + 20 NaVO3 → 2 ( 5 Na2O , V2O4 , 11 V205 ) + O2 C. Dissolution of oxygen in the molten mixture . According to Cunningham and De S ...
Other editions - View all
Common terms and phrases
70/30 copper-nickel alloy acid aerobic algae alloy aluminum Anaerobic Corrosion anodic aqueous Association of Corrosion ASTM attack Basin Saline Waters behaviour biocorrosion Biodeterioration biofilm Biofouling Biologically Induced Corrosion boiler brackish water carbon steel cathodic chemical chloride coating components concentration containing copper Corrosion Engineers corrosion potential corrosion process corrosion products corrosion rate crevice corrosion Dead Sea Dead Sea Basin depolarization deposits Desulfovibrio dissolved oxygen Dual Age effect electrochemical environment film fouling fuel H. A. Videla hydrogen sulfide immersed inhibitor ions iron sulphide laboratory layer Marine materials measurements mechanism metal surface Microbial Corrosion microfouling microorganisms mild steel molten salts NACE organisms oxide pipelines pipes piping materials pitting pitting corrosion polarization resistance present protective reaction S.C. Dexter Saline Waters Salvarezza samples Sdom Sea Basin Saline seawater soil solution stainless steel sulfate-reducing bacteria sulfur sulphate sulphide sulphur Table Tamar techniques temperature Thiobacillus tubing vanadium