1964 Exposure Test of Porcelain Enamels on Aluminum: Three Year InspectionU.S. National Bureau of Standards, 1970 - 11 pages An exposure test of porcelain enamels on aluminum was initiated by the National Bureau of Standards and the Porcelain Enamel Institute in 1964.The enamels were returned from the exposure sites to the laboratory at NBS to be measured for changes in gloss and col * or after exposures of six months, one year, and three years.Changes were found to be greatest at Kure Beach and least at Montreal and Los Angeles, with moderate changes occurring at Washington and New York.Although the boiling citric acid test is used as an acceptance test for these enamels, the correlation with color change, particularly at Kure Beach, was not as good as expected.A cupric chloride test was developed which shows an improvement in this correlation.(Author). |
From inside the book
Results 1-5 of 6
Page 2
... boiling acid solubilities were determined in accordance with ASTM ... solution of trisodium phosphate and sprinkled with calcium car- bonate , ( 2 ) rinsing ... solubility spot test ratings mils AA - A White High Two 70.1 4.5 mg / in 5.5 ...
... boiling acid solubilities were determined in accordance with ASTM ... solution of trisodium phosphate and sprinkled with calcium car- bonate , ( 2 ) rinsing ... solubility spot test ratings mils AA - A White High Two 70.1 4.5 mg / in 5.5 ...
Page 3
... acid resistance of porcelain enamels aluminum is measured by either the boiling acid solubility test [ 2 ] or by the citric acid spot test [ 3 ] . The enamels are rated by the boiling acid solubility test on the basis of weight loss per ...
... acid resistance of porcelain enamels aluminum is measured by either the boiling acid solubility test [ 2 ] or by the citric acid spot test [ 3 ] . The enamels are rated by the boiling acid solubility test on the basis of weight loss per ...
Page 8
... BOILING ACID SOLUBILITY , mg / in.2 84 2 4 6 8 10 12 14 16 18 20 20 BOILING ACID SOLUBILITY , mg / in.2 FIGURE 4. Correlation between boiling acid solubility test and color retention for the enamels exposed at ( a ) Kure Beach , ( b ) ...
... BOILING ACID SOLUBILITY , mg / in.2 84 2 4 6 8 10 12 14 16 18 20 20 BOILING ACID SOLUBILITY , mg / in.2 FIGURE 4. Correlation between boiling acid solubility test and color retention for the enamels exposed at ( a ) Kure Beach , ( b ) ...
Page 9
... boiling acid solubility test is illustrated for Kure Beach and Los Angeles in figure 4. It can be seen that at the mild site , Los Angeles , the color retention remains high regardless of the boiling acid solubility , while at the ...
... boiling acid solubility test is illustrated for Kure Beach and Los Angeles in figure 4. It can be seen that at the mild site , Los Angeles , the color retention remains high regardless of the boiling acid solubility , while at the ...
Page 10
... boiling acid solubility as indicated by the smaller residual standard deviations ( see table 7 ) for the fits of the least squares lines . Although the correlation between the color re- tention and the results of the boiling cupric ...
... boiling acid solubility as indicated by the smaller residual standard deviations ( see table 7 ) for the fits of the least squares lines . Although the correlation between the color re- tention and the results of the boiling cupric ...
Common terms and phrases
1964 Exposure Test 25 cents accordance with ASTM acid resistance acid solubility test acid spot test AG-C Angeles Montreal ASTM Book ASTM designation E-376 automatic data processing Average color retention boiling acid solubility boiling cupric chloride Book of Standards Building Science Series Bureau of Standards change in NBS citric acid spot color change color-retention data correlation between color cupric chloride test Eddy Current enamel colors Enamel Kure Beach enamel systems enamels exposed enamels included enamels on aluminum exposed at Kure gloss and color gloss range high gloss enamels initial gloss Interrelations Between Cement Kure Beach Washington low gloss enamels Medium minus the color Montreal Los Angeles National Bureau nature-tone enamels NBS units percentage gloss retained porcelain enamels Portland Cement Resistance of Porcelain RETENTION AFTER 3-YEARS retention is 100 retention of porcelain sign test Spalling specimens specular gloss spot test ratings Test of Porcelain Washington New York Weather Resistance York Montreal